Skip to main content
. 2020 Sep 21;13(18):4189. doi: 10.3390/ma13184189

Table 4.

Summary of tests to study the influence of the crack width under consideration of the observed crack-bridging behaviour.

Series Number of Specimens
Total Fibre Rupture with One-Way Full Debonding and Slippage Fibre Rupture
with Two-Way
Full Debonding
and Slippage
Complete Fibre Pull-Out Fibre Rupture in Cyclic Stage
R 11 9 2 0 -
C40-NC-200 7 6 1 0 0
C40-MC-200 10 10 0 0 0
C40-HC-200 10 6 2 2 0
C40-NC-1000 4 4 0 0 0
C40-MC-1000 10 8 2 0 0
C40-HC-1000 10 8 1 1 0
C40-NC-2000 10 10 0 0 0
C40-MC-2000 10 7 2 1 0
C40-HC-2000 10 10 0 0 0
C100-NC-200 10 6 1 3 0
C100-MC-200 10 9 0 1 1
C100-HC-200 9 9 0 0 5
C100-NC-1000 11 9 0 2 1
C100-MC-1000 11 10 0 1 6
C100-HC-1000 10 10 0 0 4
C100-NC-2000 10 7 3 0 0
C100-MC-2000 8 7 1 0 3
C100-HC-2000 8 8 0 0 3