Figure 3.

Figure 3

Structure of coatings obtained in the “pure” zinc bath on steels with different silicon content: low-silicon steel (a), Sandelin’s steel (b), Sebisty’s steel (c) and high-silicon steel (d); temperature: 450 °C, immersion time: 3 min, adapted from [36].