. 2020 Aug 27;12(9):1933. doi: 10.3390/polym12091933

Table A1.

XPS data of the C1s carbon peak from fitted Voigt profiles of PP60 before and after plasma treatment with different working gases.

Working Gas C–C/at% C–O/at% C=O/at% O–C=O/at%
Reference 96.5 3.5
Nitrogen (Ar/N2) 78.8 8.6 5.0 7.6
Oxygen (Ar/O2) 79.9 8.1 5.0 7.0
Syn. air 80.3 8.0 4.8 6.9