Published in final edited form as: Ann Biomed Eng. 2020 Apr 2;48(8):2268–2278. doi: 10.1007/s10439-020-02500-5

FIGURE 2.

FIGURE 2.

Biaxial mechanical data illustrating the (a) pressure-diameter, (b) force-pressure, and (c) circumferential stretch-stress behavior of murine infrarenal aortas exposed to 0 U/mL (control; red circles), 0.5 U/mL (blue triangles), or 10 U/mL (green squares) of porcine pancreatic elastase. Data is shown at axial stretch ratios of 1.62 and 1.2 for the control and elastase-exposed groups, respectively. All data is presented as mean values ± the standard deviation (n = 4 per group) with pressure error-bars (roughly ± 0.45 mmHg) omitted for clarity.