Skip to main content
. 2020 Aug 19;12(9):1857. doi: 10.3390/polym12091857

Figure 3.

Figure 3

(a) Elastic modulus and, (b) ultimate tensile strength comparison due to thickness effect for virgin and regrind HDPE at room temperature (RT) and 6 × 10−4 s−1 strain rate.