. 2020 Oct 16;11:5242. doi: 10.1038/s41467-020-19078-0

Fig. 5. HRTEM images and SAED patterns of S@BPCS electrode at different discharge voltages.

Fig. 5

a SAED pattern and b corresponding HRTEM at 2 V. c SAED pattern and d corresponding HRTEM at 1.65 V; e SAED pattern and f corresponding HRTEM at 1.2 V and g SAED pattern and h corresponding HRTEM at 0.8 V; mechanistic characterization of the S@BPCS electrode. i Cyclic voltammogram. j In situ X-rays diffraction (XRD) patters in the selected range of degree 2-theta (right) with first two charge–discharge profiles at a current density of 0.5 C.