. 2020 Sep 16;12(9):2103. doi: 10.3390/polym12092103

Table 1.

Direct current (DC) conductivity for the plasticized electrolyte system at room temperature.

Designation Rb (Ohm) Conductivity (S cm−1)
CSDNHP1 0.88 × 104 2.02 × 10−6
CSDNHP2 3.3 × 102 5.38 × 10−5
CSDNHP3 0.59 × 102 3.06 × 10−4