Skip to main content
. 2020 Sep 16;12(9):2105. doi: 10.3390/polym12092105

Figure 3.

Figure 3

SEM images of silk fiber surfaces. (a) Non-degummed raw silk fibers, (b–j) degummed with 0.01, 0.05, 0.1, 0.3, 0.5, 1.0, 3.0, 4.0, and 6.0 g/L papain, (k) degummed with 0.5 g/L Na2CO3, (h’) magnified image of (h). Scale bars: (ak) 20 μm, (h’) 10 μm.