Skip to main content
. 2020 Sep 16;12(9):2105. doi: 10.3390/polym12092105

Figure 6.

Figure 6

(a-1) and (a-2) SDS-PAGE patterns of regenerated SF derived from different degumming methods. (M) Molecular weight marker, (A) Na2CO3-SF, (B) 3.0 g/L papain-SF. Separating gel concentration: (a-1) 15%, (a-2) 6%. (b) Semi-quantitative statistics of molecular weight distributions (MWDs) based on SDS-PAGE patterns.