Figure 9.

Figure 9

SEM images, at different magnification, of the residues of the LbL-treated fabrics after vertical flame spread tests. 5, 10 and 20 correspond to the number of deposited bi-layers. CH = chitosan; PT = phosphorylated chitin; 0.5 and 2 are the wt. % concentrations of the biomacromolecules in the dipping baths. Reprinted with permission from [39]. Copyright 2015, Elsevier.