Skip to main content
. 2020 Oct 13;25(20):4653. doi: 10.3390/molecules25204653

Figure 3.

Figure 3

Differential Scanning Calorimetry curves of the PHA and PLA films reinforced with CNC and MF during the first heating stage (a) and during the second heating stage (b).