Table 6.
Material | E | σ | ε | Tg | Tmelt | Loss of Mech. Prop. | Total Degradation |
---|---|---|---|---|---|---|---|
(GPa) | (MPa) | (%) | (°C) | (°C) | (Months) | (Months) | |
PLLA | 3.4–4.8 | 10–100 | 2–6 | 60–65 | 170–180 | 6 | 24–67 |
PGA | 6.8–12.5 | 70–647 | min | 35–40 | 180–230 | 1–2 | 6–12 |
PLGA (D/L/PLG) 85/15-50/50 |
2 | 20–50 | 3–10 | 45–55 | - | 1–4 | 2–6 |
PCL | 0.3–0.4 | 16–23 | 300–700 | −60 | 59–64 | 0.8 | >34 |
Tg: Glass transition temperature and Tmelt: melting point.