Skip to main content
. 2020 Aug 28;12(Suppl 1):S480–S487. doi: 10.4103/jpbs.JPBS_143_20

Table 6.

Surface roughness values of IPS e.max Ceram before and after immersion in chlorhexidine mouthwash solution (in µm)

Sample no. Roughness before immersion (µm) Roughness after immersion (µm)
1 0.96 0.99
2 0.83 0.84
3 0.57 0.67
4 0.51 0.52
5 0.82 0.84
6 1.13 1.21
7 0.41 0.46
8 0.59 0.63
9 0.99 1.06
10 0.73 0.79
11 0.81 0.88
12 0.47 0.56
13 1.32 1.44
14 0.89 0.91
15 0.97 1.05
16 0.68 0.75