Surface roughness values of IPS e.max Ceram before and after immersion in simulated vomit solution (in µm)

Sample no. Roughness before immersion (µm) Roughness after immersion (µm)
1 0.72 1.39
2 0.65 1.29
3 0.81 1.69
4 0.52 1.11
5 0.49 0.98
6 0.91 1.78
7 1.27 1.97
8 1.08 1.71
9 0.68 1.07
10 0.77 1.82
11 0.87 1.63
12 0.99 1.98
13 0.59 1.07
14 0.61 1.28
15 0.74 1.41
16 0.69 0.99