. 2020 Oct 12;10(10):2011. doi: 10.3390/nano10102011

Table 2.

Magnetic properties of bare, modified and oxidized magnetite NPs.

Sample Saturation Magnetization Ms, emu/g Remanent Magnetization Mr, emu/g Coercive Force Hc, Oe
Fe3O4 (bare) 68.2 6.88 74.1
Fe3O4/HA 30.9 6.40 160
Fe3O4/HAox (harsh oxidation) 15.7 4.11 159

HA—humic acids, ox—oxidized.