Skip to main content
. 2020 Oct 9;12(10):2309. doi: 10.3390/polym12102309

Figure 4.

Figure 4

Powder x-ray diffractometer (PXRD) pattern of ZIF-8 after water immersion (ZIF-8 w) in comparison with the as synthesized ZIF-8.