Surface morphology of ZIF-8@PES prepared using different mixing ratios at high magnification. (ad) SEM micrograph of 10, 20, 30, and 40 wt %, respectively, and (eh) SEM-EDX of 10, 20, 30, and 40 wt %, respectively (Green: Zinc).