Sample Composition Processing Conditions
PLA
Content *
Cellulose Fibers
Content *
PLA 100% /
  • 170 °C for 10 min

  • 170 °C for 25 min

  • 190 °C for 10 min

  • 170 °C for 25 min

35 vol.% 65 % 35% (=10 wt.%)
55 vol.% 45 % 55 % (=20 wt.%)
68 vol.% 32% 68 % (=30 wt.%)
77 vol.% 23% 77% (=40 wt.%)