Skip to main content
. 2020 Oct 13;12(10):2343. doi: 10.3390/polym12102343

Figure 9.

Figure 9

Figure 9

Change of viscoelasticity properties of the SBR binary filler compounds by different cure temperatures: (a) tan ẟ at 60 °C, (b) G″ at 0 °C, and (c) G* at −20 °C.