Effect of silica-silane–rubber network (SSRN) or carbon black bound rubber (CBBR) on the performance change of rubber compounds with increasing cure temperature.

Item Cure Temp. Crosslink Density M100% M300% Fuel Economy Wet
Traction
Snow Traction
Increase of CB ratio Low (150 °C) G G E B B G
High (170 °C) B B G W M B
Increase of Silica ratio Low (150 °C) E E G E G W
High (170 °C) M G M G M B

E: excellent; G: good; M: moderate; B: bad; W: worst.