Skip to main content
. 2020 Oct 13;13(20):4548. doi: 10.3390/ma13204548

Figure 9.

Figure 9

Volume fraction Nbss as function (a) of Ge + Sn in heat-treated alloys and (b) of Sn/Ge in as-cast alloys. In (a) data for HT alloys, JZ1, JZ2 [46], JZ3, JZ3+ [47], with red for JZ5, green for JZ4, triangle for JZ3+, square for JZ3, blue for JZ2, and brown for JZ1. All data R2 = 0.9129, and data for Ta-containing alloys R2 = 0.942. In (b) data for cast alloys JZ2 to JZ5, red filled circles for experimental data, and blue circles for calculated data using NICE. AC = as cast, HT = heat treated.