Skip to main content
. 2020 Oct 13;13(20):4548. doi: 10.3390/ma13204548

Table 1.

Density of the as-cast (AC) alloys and area % of selected phases in the bulk of the as-cast and heat-treated (HT) alloys JZ4 and JZ5.

Alloy Density (g/cm3) Solid Solution (%) A15 (%)
JZ4-AC 7.28 ± 0.01 - 19.8 ± 3.2
7.27–7.29 17.3–23.4
JZ4-HT a - 3.3 ± 0.5 12.2 ± 2.0
2.7–3.6 10.9–14.5
JZ5-AC 6.91 ± 0.06 - 12.7 ± 1.1
6.87–7.01 11.4–13.4
JZ5-HT a - 2.3 ± 0.3 10.6 ± 0.3
2.1–2.6 10.4–10.9

a Some hafnia may be included in the measurement because the oxide exhibited the same contrast as the solid solution.