Skip to main content
. 2020 Oct 14;13(20):4564. doi: 10.3390/ma13204564

Figure 7.

Figure 7

Room temperature tensile true stress-true strain curves of Al-12Si samples fabricated with decreasing laser power (320 W–80 W) at a constant laser scan speed (1455 mm/s) in an SLM solutions SLM 250 device [68]. Copyright 2017. Adapted as per the open access policy of Taylor and Francis group (Figure 1b [68]).