Skip to main content
. 2020 Oct 14;13(20):4564. doi: 10.3390/ma13204564

Figure 8.

Figure 8

Room temperature tensile true stress-true strain curves of Al-12Si samples fabricated at a constant energy density of 55 J/mm3 with varying laser power and laser scan speed in an SLM Solutions SLM 250 device [68]. Copyright 2017. Adapted as per the open access policy of Taylor and Francis group (Figure 1a [68]).