Skip to main content
. 2020 Oct 14;13(20):4564. doi: 10.3390/ma13204564

Figure 33.

Figure 33

Evolution of pores in SLM-processed AlSi10Mg as a function of laser scan speed: (a) 250 mm/s, (b) 500 mm/s, (c) 750 mm/s and (d) 1000 mm/s [76]. Copyright 2014. Adapted from Elsevier Science Ltd. (Figure 5 [76]).