Skip to main content
. 2020 Oct 14;13(20):4564. doi: 10.3390/ma13204564

Figure 37.

Figure 37

AlSi10Mg single tracks showing the variations in the shape of the fusion line and the defect formation as a function of laser scan speed (a) 250 mm/s, (b) 500 mm/s and (c) 750 mm/s [167]. Copyright 2015. Adapted with permission from Elsevier Science Ltd. under the license number 4803731331814 (Figure 9 [167]), dated 7 April 2020.