Table 5.

The unconfined specimens’ dimensions and their corresponding test method.

Specimen Description (Test Method) Dimension Perlite Ratio in Weight (%)
SPC HESC with perlite
(ASTM C39/C39M-18)
Φ10 cm × 20 cm 0; 10; 20; 30
SPCC HESC with perlite confined by CFRP (ASTM C39/C39M-18) Φ10 cm × 20 cm
SPTC HESC with perlite under elevated temperature (ASTM C109/C M109-02) 5 cm × 5 cm × 5 cm