Designed different perlite ratios of the thermal-insulating material specimens.

Specimen Perlite Ratio in Weight (%) Perlite (g) HESC (g) Water (g)
SPC0 0 0 2000 700
SPC10 10 200 1800 630
SPC20 20 400 1600 560