. 2020 Oct 15;13(20):4587. doi: 10.3390/ma13204587

Figure 4.

Figure 4

Results of total and open porosity calculations based on micro-CT data for the CH/SHA matrix nanocomposites modified with 1, 5, and 10 wt.% of 2D Ti3C2Tx MXene flakes (a). For comparison, results for CH composites (with no sodium hyaluronate) are shown in (b).