Figure 2.

Figure 2

(a) SEM image depicting the morphology of fabricated PVA SPTF-HA; and (b) magnified image of PVA SPTF-HA with helicoidally arranged PAN fibers. Here, 13 helicoidally arranged PAN fibrous layers with 45° ± 3° offset angle are embedded layer by layer in 5 wt% PVA/H2O solution and later dried to fabricate PVA SPTFs.