Properties of commonly used crystals for PET scanners

BGO GSO LSO LYSO
Density (g/cm3) 7.1 6.7 7.4 7.4
Attenuation length (mm) 10.4 14.1 11.4 11.8
Light output (photons/MeV) 9000 8000 30,000 30,000
Light decay time (ns) 300 60 40 40