Table 1. Firing procedure of opaque and dentin porcelain.
| Porcelain | Firing | Preheating (°C) | Drying (min:s) | Heating Rate (°C/min) | Final Temp. (°C) | Holding (min) |
|---|---|---|---|---|---|---|
| VMK Master | Opaque | 500 | 5:38 | 80 | 950 | 1 |
| Dentin | 500 | 7:49 | 55 | 930 | 1 | |
| Glaze | 500 | 5:15 | 80 | 920 | 1 |
| Porcelain | Firing | Preheating (°C) | Drying (min:s) | Heating Rate (°C/min) | Final Temp. (°C) | Holding (min) |
|---|---|---|---|---|---|---|
| VMK Master | Opaque | 500 | 5:38 | 80 | 950 | 1 |
| Dentin | 500 | 7:49 | 55 | 930 | 1 | |
| Glaze | 500 | 5:15 | 80 | 920 | 1 |