Skip to main content
. 2020 Oct 28;15:8311–8329. doi: 10.2147/IJN.S271159

Figure 3.

Figure 3

XRD patterns of pristine graphite, GO, GO-PF, NanoGO, and NanoGO-PF, along with PF as control measured at 30 kV and 30 mA, with a scanning rate of 2°/min and 2ϴ angles ranging from 2–60°.