Table 1. Step-growth polymerization (polyaddition) of tri-Boc spermine and 1,4-butanediol diacrylate and deprotection of the resulting polymer.

Polymer Solvent Time (h) Yield (%) Mn(Da) Ð Protonable unit
P(BSpAE) 5[a] neat 15 83 3600[c] 1.73[c] 350
P(SpBAE) 6[b] DCM 2 63 3800[d] / 186
[a]

reaction conditions: neat, 120 °C, overnight, the molar ratio of spermine and 1,4-butanediol diacrylate is 1:1.

[b]

reaction conditions: polymer 5, TFA, DCM, room temperature, 2 h.

[c]

Mn and Ð was assessed via SEC (measurement relative to polystyrene and in chloroform at 30 °C).

[d]

molecular weight was calculated on the basis of SEC of polymer 5 (Figure S3) and the theoretical chemical structure of polymer 6.