Table 3.

Comparison of the measured crystallinity index for CNCs using various techniques.

Cellulose source XRD* NMR 380-Raman 93-Raman References
MCC 84 NA 77 68 68,81
Cotton 92 75 77 68 57,81
Wood 80–89, 90, 72 60 56 46 70,81,82
Tunicate 91, 95 80, 94 70 93 34,81
Wood 66, NA 56 46 This work
Tunicate 75 NA 68 96 This work

NA is not available | * For wood, wide range attributable to varying methods used to calculate crystallinity.