(a) PCL–PEG–PCL hydrogels were formed by increasing PEG block MW to 4 or 8 kDa; (b) scanning electron microscope (SEM) micrograph of a dehydrated polymer sample displays the 3D structure of the polymer without heating to form a gel; (c) the gel network resulting from heating at 50 °C for one minute.