Alg/T20 slurry Yield stress (Pa) G’ (Pa)
Prepared with 0.90 wt% NaCl solution
 Before heating 93.4 ± 5.1 249.5 ± 42.4
 5.0 wt% glycerol addition after heating No crossover point (yield stress > 100 Pa)
 100 wt% glycerol addition after heating
 15.0 wt% glycerol addition after heating
Prepared with 0.45 wt% NaCl solution
 Before heating 18.1 ± 0.7 160.8 ± 1.0
 7.5 wt% glycerol addition after heating No crossover point (yield stress > 100 Pa)
 12.5 wt% glycerol addition after heating