Skip to main content
. 2020 Nov 4;25(21):5130. doi: 10.3390/molecules25215130

Figure 3.

Figure 3

HSM micrographs for PU at different temperatures: (A)—PU at 25 °C; (B)—PU at 25 °C—back cooled product; (C)—PU at 245 °C—melting starts; (D)—PU at 250 °C—partially melted; (E)—PU at 255 °C—partially melted; (F)—PU at 260 °C—melted. The magnification in the photographs was 59.7×.