Skip to main content
. 2020 Oct 28;13(21):4821. doi: 10.3390/ma13214821

Figure 6.

Figure 6

XPS C1s high-resolution spectra of (a) blank chitosan and chitosan/Ag NP composites prepared using a plasma-solution system with (b) the liquid anode, and (c) the liquid cathode. Treatment time, 30 min.