Mean values (± standard deviations) of MC at the start of the measurement, bulk density of wood samples (ρb), tan δ response in the whole range of temperatures and average values of E’, E’’ and tan δ at 25 °C.

Wood Type/
Dynamic Force (N)
ρb
(g cm−3)
Tan δ Response (°C) E’
[MPa]
at 25 °C
E” [MPa]
at 25 °C
Tan δ
at 25 °C
γ βwet β
CE (0.5) 0.70 ± 0.02 −103 ± 8 −6 ± 11 > 417.7 ± 93.1 16.0 ± 1.4 0.040 ± 0.008
AE (0.2) 0.55 ± 0.08 −86 ± 6 - 42 ± 7 86.9 ± 16 4.0 ± 1.6 0.046 ± 0.004

Note > indicates that a peak was visible above the 40 °C threshold selected as cut off point for formal presentation and analysis.