Temperature change (°C) of FA-G and FA-G/AuNPs composite scaffolds after 10-min laser irradiation. Data represent mean ± SD.

1.3 W/cm2 1.4 W/cm2 1.5 W/cm2 1.6 W/cm2
FA-G 4.60.2 5.80.1 7.60.2 9.00.5
FA-G/R40 18.80.2 20.40.1 22.30.2 23.90.3
FA-G/R70 28.70.1 30.80.2 33.00.3 35.10.4
FA-G/R110 21.80.1 23.30.1 24.90.5 26.30.3
FA-G/S40 18.10.3 20.10.2 22.20.3 24.00.2
FA-G/S70 19.40.3 21.70.2 24.00.1 26.10.1
FA-G/S110 19.30.1 21.60.2 23.10.2 25.00.1