Fig. 3. STRAP process separates PE, EVOH, and PET mixtures.

Fig. 3

(A) Process schematic for deconstructing an Amcor Evolution multilayer film into its constituent resins using the STRAP process. (B) Photographs of the Evolution film and the recovered resin using the STRAP process in (A). The mass balance for this process is 100.44 wt % with respect to the initial mass of the evolution film, with an SE of ±1.39 wt %. Photo credit: Theodore W. Walker, University of Wisconsin-Madison. (C) Photographs of comingled plastic resin beads consisting of 7:2:2 PE, EVOH, and PET and the recovered resins using the same procedure in (A). The mass balance for this process is 99.40 wt % with respect to the initial mass of the physical mixture, with an SE of ±0.19 wt %. Photo credit: Theodore W. Walker, University of Wisconsin-Madison.