Skip to main content
. 2020 Oct 22;12(11):2434. doi: 10.3390/polym12112434

Figure 2.

Figure 2

Kinetic analysis of polylactic acid (PLA) degradation. (a) Number average molecular weight (Mn) of PLA after treatment with sub-critical water, according to reaction time and temperature and (b) analysis of the reduction in molecular weight due to sub-critical water, using a first-order equation.