. 2020 Oct 22;12(11):2436. doi: 10.3390/polym12112436

Figure 3.

Figure 3

The contact angles and aging of unmodified FEP (pristine) and FEP foils modified at 8 W and 240 s and then immersed in polymer solution containing 1, 2, or 3 g of PLLA.