Skip to main content
. 2020 Oct 23;12(11):2452. doi: 10.3390/polym12112452

Figure 7.

Figure 7

(a) PCFC and (b) TGA curves (in nitrogen) of GDP treated PP, PLA, flax, flax/PP, and flax/PLA.