SEM micrograph of unfilled epoxy network (left), epoxy/diaminodiphenylsulfone (DDS)/MWNT nanocomposite (0.7 wt %) after a 5 h dispersion with Rayneri (right) and epoxy/DDS/MWNT nanocomposite (0.7 wt %) after a dispersion with 3 roll-mill calander (below).