. 2020 Oct 29;12(11):2530. doi: 10.3390/polym12112530

Figure 15.

Figure 15

G’ band shift as a function of the compression strain of DGEBA/DDS/MWNT nanocomposite (0.7 wt %) and of two different dispersion states (DD = 4.9 and DD = 74.5).