. 2020 Nov 10;13(22):5068. doi: 10.3390/ma13225068

Figure 14.

Figure 14

SEM micrographs showing the tensile fracture surface of the F-SP-T-2 specimen: (a) low-scale SEM photograph of near initial fracture; (b) magnification view of rectangle ① in (a); (c) magnification view of rectangle ③ in (b); (d) magnification view of rectangle ② in (a); and (e) magnification view of rectangle ④ in (d).