Skip to main content
. 2020 Nov 10;13(22):5070. doi: 10.3390/ma13225070

Figure 3.

Figure 3

SEM micrograph (in BSE) of the coarse-grained microstructures of Fe-10Al-4Y2O3 new-generation ODS alloy after secondary recrystallization hot rolled at (a) 840 °C, (b) 900 °C, (c) 960 °C, and (d) 1020 °C.