Figure 6

Summarizing results creep at 1100 °C of the most promising heats Fe-10Al-4Y2O3 rolled at 900 °C and 930 °C and Fe-9Al-14Cr-4Y2O3 rolled at 930 °C, (a) dependences of time to fracture on applied stress, (b) dependences of secondary creep rate on applied stress, (c) dependences of ductility on applied stress, and (d) longest creep curve of the studied heats.